CHANGZHOU FENGDAFANGFEI INDUSTRY CO.,LTD.
|
Gold Index: 4064
Place of Origin: | Zhejiang, China (Mainland) |
Add to My Favorites | |
HiSupplier Escrow |
Specifications:
Test | Unit | Standard/ Guaranted |
Mass per unit area | g/ | 160/152.0 |
thickness | mm | 0.80/0.68~0.92 |
width | m | 3.8 |
Max. Tensile strength (MD) | KN/m | 12/10.2 |
Max. Tensile strength (CD) | KN/m | 11/9.2 |
Elongation at Max. tensile strength (MD) | % | 30.0/25 |
Elongation at Max tensile strength (CD) | % | /35.0/27 |
CBR bursting strength | KN | 1.8/1.5 |
shrinkage(MD) 200 | % | ≤1.7 |
shrinkage(CD)200 | % | ≤0.1 |
Elongation 3% Tensile strength(MD) | KN/m | 5/4.5 |
Elongation 15%Tensile strength(MD) | KN/m | 9/8.1 |
Elongation 3% Tensile strength(CD) | KN/m | 3.6/3.24 |
Elongation 15%Tensile strength(MD) | KN/m | 6.4/5.76 |
Trapezoid tearing strength | KN | 0.2 |
bitumen oil adsorption | L/ | 0.8-1.2 |
Melting point | 256 |
Description:
by the condition of bitumen road , many investigation show that :common disease of bitumen concrete road is crack ,rut and basic softening .if we prevent above disease effective,it will be more safety and comfortable for driving
The main reason of above disease is as follows:
1. expand with heat and contract with cold because the temperature
2. ageing of bitumen and elasticity decline of surfacing
3. substrate has crack and horizontal fall head
4. material which used and construction method ,etc
According to the cracking of bitumen concrete road ,when we add the surface on the before road or semi-rigid surface , we can use the high performance polyester spunbond between new surfacing and old surfacing , then we can prevent above disease .